Historical

SAE AMS 5596K-2007 (SAE AMS5596K-2007)

Nickel Alloy, Corrosion and Heat Resistant, Sheet, Strip, Foil, and Plate 52.5Ni 19Cr 3.0Mo 5.1Cb (Nb) 0.90Ti 0.50Al 18Fe Consumable Electrode or Vacuum Induction Melted, 1775\mDF (968\mDC) Solution Heat Treated


This specification covers a corrosion and heat resistant nickel alloy in the form of sheet, strip, foil, and plate. These products have been used typically for parts requiring resistance to creep and stress-rupture up to 1300 \mDF (704 \mDC) and oxidation resistance up to 1800 \mDF (982 \mDC), particularly those parts which are formed or welded and then heat treated to develop desired properties, but usage is not limited to such applications.


CONTENT PROVIDER
Society of Automotive Engineers [sae]

Others Also Bought
Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings, Extrusions, and Rings 62Ni 21.5Cr 9.0Mo 3.65Cb (Nb) ...
Heat Treatment of Steel Raw Materials
Document History
Included in Packages
This standard is not included in any packages.
Amendments & Corrections
We have no amendments or corrections for this standard.