Historical

TAPPI T 818 cm-07

Ring crush of paperboard


The ring crush test correlates with edgewise compression strength of paperboard (1). This method is intended for paperboard between 0.28 mm (0.011 in.) and 0.51 mm (0.020 in.) thick. It may be used with less reliability for paperboard as thin as 0.18 mm (0.007 in.), and as thick as 0.76 mm (0.030 in.). The short span compression test, TAPPI T 826 “Short Span Compressive Strength of Paperboard,” measures edgewise compressive strength over a broader range of thickness. Ring crush is also measured in TAPPI T 822 “Ring Crush of Paperboard (Rigid Support Method),” which uses a rigid platen compression machine instead of the flexing beam of this method.


CONTENT PROVIDER
Technical Association of the Pulp and Paper Industry [tappi]

Others Also Bought
Ring crush of paperboard (rigid support method)
Fluted edge crush of corrugating medium (rigid support method)
Short span compressive strength of containerboard
Document History
Revised By:
Included in Packages
This standard is not included in any packages.
Amendments & Corrections
We have no amendments or corrections for this standard.